MIM 4605 Case Hardened
Material Properties Kinetics
Typical 2
Ultimate Strength (KSI) -
Yield Strength (KSI) -
Elongation (% in 1") -
Reduction in Area (%) -
Surface Finish (Ra) 40
Impact Energy (ft-lbf)1 -
Macro Hardness (R15N) 88.3
Sintered Density (g/cm3) 7.6

1Test method uses 1/2 sized un-notched charpy bar.
2 Typical values at a hardness of 47 HRC. Higher hardness and strength characteristics can routinely be obtained through varying Quench and Temper conditions

 

Material Description:
Low alloy steel, carbon, nickel, molybdenum. A multipurpose, economical material that offers various strength, hardness and wear resistance properties depending on whether it is heat treated and which heat treat process is used. Magnetic. Can be plated or coated for corrosion resistance. Used by a very wide range of industries including automotive, consumer products, firearms, power hand tools, structural and applications where good strength, hardness and wear resistance are required.


 
Material Composition (%):
 
Fe Ni Mo C (Max) Si (Max)
Balance 1.5-2.5 0.2-0.5 0.4-0.6 1.0

 
Click Here to Print This Page

 
About Our Company | Metal Injection Molding | Application Review | Request a Quote | Materials & Properties | What's New | Employment Opportunities | Contact Us | File Transfers | MIM Design Guide | Ask a PIM/MIM Expert a Question | Climax Engineered Materials | Home

Copyright © 2003 Kinetics. All Rights Reserved. Site designed and hosted by The Worx Group. Email the webmaster.